I am working on a project with a very tight deadline. Has anyone used Fine Silver as an inclusion or next to Bulls Eye White? Does the white react oddly to the silver like the French Vanilla does?
As always, thank you for sharing your experience.
Melissa Terman
Lou_Ohio
Posts: 8 Joined: Mon Mar 10, 2003 10:49 pm
Location: Highland Heights , Ohio
Post
by Lou_Ohio » Sun Aug 24, 2003 12:57 pm
I have used this combination ( opal white & Fine silver ) without a problem .
Lou
Dani
Posts: 493 Joined: Mon Mar 10, 2003 3:17 pm
Contact:
Post
by Dani » Sun Aug 24, 2003 1:25 pm
How do you prevent silverstain (yellow halo-ing)? Thanks.