PDV nuggets and slices

Posted: Sat Dec 15, 2007 9:16 am
by Lisa Sharik
Hi
I tried to make my first large piece of pate de verre since class with Marc an Ellen and it didn't turn out as I wanted. So since I had some nice looking glass in an ugly shape I sliced and diced and cold worked it till I took off half of one of my fingernails and abraded both my thumbs #-o
The results are below. I really like the nuggets they remind me of watermelon tourmaline. I sold several of them on Etsy already.
I did get my first large piece fired and I plan to spend the morning trying to get the plaster out and hope that my bottom glass is thick enough. It is a rectangluar vessel done in a one piece mold. I'll post picture of it when it's out.
lisa
Image
Image
Image
Image

Re: PDV nuggets and slices

Posted: Sat Dec 15, 2007 9:40 am
by Lib
Lemonade from lemons Lisa- those are pretty. I especially like the polished "crystals" in the top pix. Bummer about the fingernail though... she says, looking at her still mis-shapen fingers from the table saw incident. I guess they'll never be nice and round and symettrical again, poo.

Re: PDV nuggets and slices

Posted: Sat Dec 15, 2007 9:44 am
by Tom White
That is making good use of the glass you had. The crystal shapes do remind me of tourmaline. If I see Ellen today I will remind her to look at this forum to see your pictures.

Best wishes,
Tom in Texas

Re: PDV nuggets and slices

Posted: Sat Dec 15, 2007 2:23 pm
by Deb Lewis
Those are very attractive! I really like the teeny bubbles from the PDV.

I don't imagine many of us have any fingernails 8-[