Re: Help with Black Cupric Oxide?

Post by Lodahl Art Glass »

thank you Rosanna. Could you tell me how high you fired it? I fired 4 tiles and was real careful about not putting any tin sides against the oxide. Maybe the firing schedule I used wasn't enough heat?