Page 1 of 1
BE Reactive Color Chart?
Posted: Fri Jan 16, 2004 7:45 pm
by KellyG
Did a search in archives, but couldn't find info there.
Does anyone have or know where I can get a complete list of all BE reactive colors. I have a partial list from a hi-fire class, but I've seen reactions to colors not listed on my chart.
BTW, just out of curiosity, do spectrum colors react like BE?
Tiredofsurprisesgirl.
Posted: Fri Jan 16, 2004 7:46 pm
by Brock
Bullseye will give you a list, they've published it before. Brock
Posted: Fri Jan 16, 2004 7:59 pm
by KellyG
If it's the "Information courtesy of Mary Kay Nichie", I have that, but it's incomplete. There's no date on it, so I don't know if it's the most recent.
I'll contact BE tomorrow. Just hoping that a list had been published on the web somewhere.
Still curious about Spectrum color reactivity.
Thanks ...K
Posted: Fri Jan 16, 2004 8:10 pm
by Paul Tarlow
KAG wrote:If it's the "Information courtesy of Mary Kay Nichie", I have that, but it's incomplete. There's no date on it, so I don't know if it's the most recent.
I'll contact BE tomorrow. Just hoping that a list had been published on the web somewhere.
Still curious about Spectrum color reactivity.
Thanks ...K
All colored glass is subject to reactions based on the chemicals chosen by the manufacturer to achieve the specific color.
- Paul
Posted: Fri Jan 16, 2004 9:07 pm
by Brad Walker
Posted: Fri Jan 16, 2004 10:07 pm
by KellyG
Thanks Brad, great link. I didn't search old archives. Apparently, there's a wealth of info there.
I'm gonna print this one
...Kelly
Re: BE Reactive Color Chart?
Posted: Sat Jan 17, 2004 9:14 am
by Barbara Muth
KAG wrote:Did a search in archives, but couldn't find info there.
Does anyone have or know where I can get a complete list of all BE reactive colors. I have a partial list from a hi-fire class, but I've seen reactions to colors not listed on my chart.
BTW, just out of curiosity, do spectrum colors react like BE?
Tiredofsurprisesgirl.
The safest thing to do is test! You may find interesting ways to capitalize on the reactions.
Reactionmadgirl