Page 1 of 1
Got Free Rods and Glass
Posted: Sun Jun 17, 2012 5:57 pm
by glass-lady
Someone gave me a whole load of glass rods, pellets, curly pieces, e.g., all supplies from a lampworker but no idea what COE. I took a one day lampworking class several months ago where we had a super nice torch set-up. Lampworking will be 4th in what I like to do, with glass painting/fusing #1, stained glass #2, and oil painting #3. Would like some recommendations on what type of torch set-up to buy that would work decently at a hobbiest level at a reasonable cost. Thank you all so much.
Re: Got Free Rods and Glass
Posted: Sun Jun 17, 2012 8:01 pm
by Jeanne
http://www.lampworketc.com/
What warmglass.com is to fusing - lampworketc.com is to working with the torch. Everything you want and need to know is there. You'll then be able to decide what's best for you. Happy torching!
Re: Got Free Rods and Glass
Posted: Sun Jun 17, 2012 8:15 pm
by Lynn g
You could start off with a Hot Head torch and Mapp gas. Then get a more sophisticated set-up if you decide you like torchworking.
Re: Got Free Rods and Glass
Posted: Sun Jun 17, 2012 8:42 pm
by Barry Gitelson
I have a hot head that is hooked up to a five gallon LP tank and that works fine for me.
Re: Got Free Rods and Glass
Posted: Sun Jun 17, 2012 11:08 pm
by glass-lady
Thank you all very much. I went with the Hot Head because it seemed to be at the non-killer level of investment for something that may be a passing fancy. Thank you very much for the site link, that will prove useful.