slumping

This forum is for questions from newcomers to kiln-forming.

Moderator: Tony Smith

Post Reply
KissMyGlass
Posts: 3
Joined: Mon May 07, 2012 11:53 pm

slumping

Post by KissMyGlass »

I have a mask that I slumped that didn't get completely finished. Can I put it back in and redo it and if so at what temperature.
Marla
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Re: slumping

Post by Brock »

Go up to your slumping temp and hold longer. Look.