Post by Beau Lyons »

Is there such a product as float glass dichroic, and where can i purchase it
Babette (Shawn)
Posts: 103
Joined: Fri Feb 05, 2010 4:11 pm
Location: Chico California
Contact:

Re: dichroic COE82

Post by Babette (Shawn) »

“Art washes away from the soul the dust of everyday life.”
― Pablo Picasso
Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: dichroic COE82

Post by Valerie Adams »

I believe C&R Loo also sells it.
rosanna gusler
Posts: 730
Joined: Mon Mar 10, 2003 2:22 pm
Location: wanchese north carolina
Contact:

Re: dichroic COE82

Post by rosanna gusler »

cbs dichroic rosanna
artist, owner of wanchese art studio, marine finisher
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: dichroic COE82

Post by Bert Weiss »

Remember that float glass is a commodity whose manufacturers care nothing about fusing compatibility. Even published COE numbers are an average. If you want truly compatible float dichroic, have it coated with your own base glass.

Here is a link for Schott in the USA. I imagine they have an Aussie site as well. This glass is inexpensive enough that it is used for large expanses of building facades.
http://www.us.schott.com/architecture/e ... arima.html

Also remember that dichro pops best when backed with black. You can supply the black with vitreous onglaze colors.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Judd
Posts: 295
Joined: Mon Sep 01, 2003 9:45 am
Location: Arkansas

Re: dichroic COE82

Post by Judd »

You could try using dichro slide papers. They work, but I've found the dichroic coating can look washed out on some floats.

http://www.fusionheadquarters.com/Searc ... rch=dichro
Babette (Shawn)
Posts: 103
Joined: Fri Feb 05, 2010 4:11 pm
Location: Chico California
Contact:

Re: dichroic COE82

Post by Babette (Shawn) »

You can send your own float glass to CBS and they will coat it for you. This way you can make sure the glass is from the same source and it will be compatable. *Not so easy or economical from Australia.
“Art washes away from the soul the dust of everyday life.”
― Pablo Picasso
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: dichroic COE82

Post by Bert Weiss »

Try casting broken tempered low E glass. You have to use plenty of heat to get it to stick to itself.