removing bubbles
Posted: Wed Dec 26, 2012 10:11 pm
With clear casting using Resins, a method to remove bubbles is to saturate the surface of the liquid resin with Carbon Dioxide, CO2.
I do not know how it works but it does work.
Has anyone tried infusing CO2 into the kiln to remove bubbles from the hot glass.