base glass question
Posted: Fri Apr 26, 2013 7:02 am
Hi
I think I know the answer to this question but I want to check before I proceed..truly a newbie question
I always use one full piece of glass as my base glass for the blank if I am not using a clear cap on top of a design.
However, most of my glass is 10 X 10, less when I cut off the rolled edge. I know I can buy larger pieces of glass & will do that in the future.
Any issues I need to consider when to make a base of white opaque for a 11- 1/2 X 5 - 1/2 rectangle that I plan to design stacks on top of?
I assume the two pieces of white opaque will fuse together fully and not leave a line.
Also, same question if using a clear cap?
If I was not just a weekend fuser, I'd have more time for experiments and work out some of the answers to my questions.
Thanks for the advice.
Susan
I think I know the answer to this question but I want to check before I proceed..truly a newbie question
I always use one full piece of glass as my base glass for the blank if I am not using a clear cap on top of a design.
However, most of my glass is 10 X 10, less when I cut off the rolled edge. I know I can buy larger pieces of glass & will do that in the future.
Any issues I need to consider when to make a base of white opaque for a 11- 1/2 X 5 - 1/2 rectangle that I plan to design stacks on top of?
I assume the two pieces of white opaque will fuse together fully and not leave a line.
Also, same question if using a clear cap?
If I was not just a weekend fuser, I'd have more time for experiments and work out some of the answers to my questions.
Thanks for the advice.
Susan