I just got some stainless steel bowls to use a molds. I am trying to get Primo Primer to stick. I sanded the bowls, cleaned, heated to 500, and applied primo.
Couple questions.
1. I assume I put 3-5 coats on. Do I need to heat every time to 500? I kept applying coats while it was cooling, It appears I am getting coverage, but I have not fired yet.
2. I get some pooling in the base. The pooling crusts up, and looks a bit unappealing. Any way to resolve this?
3. Is there an alternative method/primer?
Thanks.