coral bowls
Posted: Wed Dec 11, 2013 5:50 pm
I want to make a couple of small "coral" bowls. The tutorial I found used stainless bowls for shaping. Could I use my ball molds and slump or is there something about the spidery construction of these that wants to drape instead of slump? Of course these are for gifts that I need next week.