Page 1 of 1
silver and glass
Posted: Mon Mar 24, 2014 10:00 am
by Miriam Silburt
Can you fire silver with glass?
Re: silver and glass
Posted: Mon Mar 24, 2014 10:15 am
by Barry Kaiser
Yes, but it does depend on the thickness of the silver and the glass it is fused with (reactivity)
I screen print silver slip all the time on to BE1401.
Difficult to cap.....yellows.
Re: silver and glass
Posted: Mon Mar 24, 2014 6:04 pm
by lorimendenhall
if you use fine silver it will stay bright silver colored. if you use sterling silver it turns ugly. I embed fine silver hangers into pendants all the time.
Re: silver and glass
Posted: Tue Mar 25, 2014 4:58 pm
by JestersBaubles
Make sure to take into considerations the reactions due to the silver. You might want to look at a blog post I did on Bullseye reactive glass:
http://jestersbaubles.blogspot.com/2014 ... glass.html
Dana W.