Post by Emily Will »

I knew that my edge matches were not perfect when I laid out this
circle of glass, but I thought that they would fuse together to deal with
the irregularities. But that did not happen as evidenced by the "black" lines
where the pieces join in the middle. So, my question is did I not hold the
temperature at the fusing point long enough, and can I go back and refuse it
to get a better result. Or, is this the best it will be and re-fusing won't help?

All suggestions are very welcome. I'd like to improve my techniques.

Thanks,
Emily
Attachments
BowlBlank.jpg
Marty
Posts: 860
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Perfecting this fused bowl-to-be

Post by Marty »

Re-fusing it will not make a difference.
Frankly, I think it's pretty good the way it is. Slump it, give it away and make another. And another.
vblue
Posts: 98
Joined: Sun Mar 09, 2003 11:05 pm
Location: Texas

Re: Perfecting this fused bowl-to-be

Post by vblue »

I agree with Marty in that it is pretty good the way it is. I really like the color combinations and the design....simple but pretty.
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: Perfecting this fused bowl-to-be

Post by Havi »

Me too. [Agree with Marty]




Havi
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
David Jenkins
Posts: 174
Joined: Wed Apr 29, 2009 10:35 pm
Location: Cypress, Texas

Re: Perfecting this fused bowl-to-be

Post by David Jenkins »

If this picture is of the results of the first fuse, I'm impressed by how well you matched the outside curves on the individual pieces.