Page 1 of 1
Clear frit
Posted: Tue Apr 08, 2014 9:32 pm
by Shelley Lewis
What's the difference between clear frit and water clear frit?
Re: Clear frit
Posted: Tue Apr 08, 2014 10:07 pm
by charlie
different glasses. water clear is more transparent than clear.
Re: Clear frit
Posted: Wed Apr 09, 2014 2:44 am
by Morganica
Usually the water clear (or crystal clear) is more colorless than the regular clear. It can make a difference, especially when you're mixing colors. Otherwise, they're pretty much interchangeable.
Re: Clear frit
Posted: Wed Apr 09, 2014 8:06 am
by Shelley Lewis
Thanks!
Re: Clear frit
Posted: Thu Apr 10, 2014 5:38 pm
by jim simmons
You can really tell the difference if your piece is fairly thick as in a casting.
Jim
charlie wrote:different glasses. water clear is more transparent than clear.