I am wanting to attach fused glass tiles to stainless steel or aluminum after using a dremel tool on the metal. Any suggestions on what to use. Also, thinking about trying to put something behind the glass to add some depth. Also, looking for suggestions on what to put on the back so it can be hung.
Thanks.
Deb
Attaching glass to stainless steel
Moderators: Brad Walker, Tony Smith
Re: Attaching glass to stainless steel
ge silicone 2. don't forget to let sit untouched for 24 hours as a minimum
-
- Site Admin
- Posts: 1489
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Attaching glass to stainless steel
And be sure to use a fresh tube.charlie wrote:ge silicone 2. don't forget to let sit untouched for 24 hours as a minimum
-
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Attaching glass to stainless steel
The depth thing comes when the glass is not in contact with the metal. So put the silicone around the perimeter making sure the glass does not touch the metal. Light will go through and bounce back.
Another good adhesive is VHB tape. VHB stands for very high bond. Letting it sit for up to 3 days will help develop strength.
Another good adhesive is VHB tape. VHB stands for very high bond. Letting it sit for up to 3 days will help develop strength.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Re: Attaching glass to stainless steel
I am thinking of using plexiglass to attach fused glass to Aluminum. For the back, looking at different stand off systems. Any suggestions on what type might be good?