CAN I FUSE W/ NICHROME WIRE???

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
jewelme
Posts: 1
Joined: Tue Feb 17, 2004 8:45 pm

CAN I FUSE W/ NICHROME WIRE???

Post by jewelme »

I'm doing a big fused glass school project with 50 kids to raise funds. We are creating some large wind chimes and need a way to connect all the chimes. I thought I would use nichrome wire but am not sure if it is compatable with Bullseye. I would be so thankful for an answer or if anyone has a better solution for connecting the pieces.... I have used copper before but it muddied up the glass around where I used it so I didn't want to go that route again. Many Thanks!!!... Regina
jim simmons
Posts: 478
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

Re: CAN I FUSE W/ NICHROME WIRE???

Post by jim simmons »

jewelme wrote:I'm doing a big fused glass school project with 50 kids to raise funds. We are creating some large wind chimes and need a way to connect all the chimes. I thought I would use nichrome wire but am not sure if it is compatable with Bullseye. I would be so thankful for an answer or if anyone has a better solution for connecting the pieces.... I have used copper before but it muddied up the glass around where I used it so I didn't want to go that route again. Many Thanks!!!... Regina
Yup, You sure can.
Jim
dee
Posts: 302
Joined: Tue Mar 11, 2003 5:20 pm
Location: Atlanta GA
Contact:

Re: CAN I FUSE W/ NICHROME WIRE???

Post by dee »

jewelme wrote:I'm doing a big fused glass school project with 50 kids to raise funds. We are creating some large wind chimes and need a way to connect all the chimes. I thought I would use nichrome wire but am not sure if it is compatable with Bullseye. I would be so thankful for an answer or if anyone has a better solution for connecting the pieces.... I have used copper before but it muddied up the glass around where I used it so I didn't want to go that route again. Many Thanks!!!... Regina
nichrome is great for what you want to do and won't muck up the glass
D
Dee Janssen
Unicorn's Creations Studio
http://ucjewelry.com
dee@ucjewelry.com
Kathie Karancz
Posts: 137
Joined: Wed Mar 12, 2003 3:49 pm
Location: Calgary, Alberta, Canada
Contact:

Post by Kathie Karancz »

What the heck is nichrome wire and where do I buy it??
:oops: :?
Kathie Karancz
Tribal Turtle
Victoria, British Columbia
http://www.tribalturtle.com
dee
Posts: 302
Joined: Tue Mar 11, 2003 5:20 pm
Location: Atlanta GA
Contact:

Post by dee »

Kathie Karancz wrote:What the heck is nichrome wire and where do I buy it??
:oops: :?
http://www.mcmaster-carr.com

it's high temp hard wire....
D
Dee Janssen
Unicorn's Creations Studio
http://ucjewelry.com
dee@ucjewelry.com
Post Reply