Has anyone successfully used the Sharpie paint pens in the kiln? (not the permanent marker type.)
Thanks,
Vernelle
Sharpie paint pens
Moderators: Brad Walker, Tony Smith
-
Aglassygirl303
- Posts: 47
- Joined: Sun Nov 08, 2009 10:08 pm
Re: Sharpie paint pens
Yes. I love them. The Oil Based ones. I made 35 Red Cardinals and offered people personal names on them. They came out beautifully. I used the extra fine point
-
Georgia Novak
- Posts: 28
- Joined: Wed Jun 04, 2003 2:54 am
Re: Sharpie paint pens
How high did you fire the paint from the pens?
Re: Sharpie paint pens
I tried the silver and gold pens. The gold turned dark but the silver was okay. I took it to around 1500. Have you tried any other colors?
-
Aglassygirl303
- Posts: 47
- Joined: Sun Nov 08, 2009 10:08 pm
Re: Sharpie paint pens
I used the gold after I fired the piece
-
Aglassygirl303
- Posts: 47
- Joined: Sun Nov 08, 2009 10:08 pm
Re: Sharpie paint pens
I used the gold after I fired the piece