Has anyone successfully used the Sharpie paint pens in the kiln? (not the permanent marker type.)
Thanks,
Vernelle
Re: Sharpie paint pens
Posted: Wed Dec 17, 2014 1:11 am
by Aglassygirl303
Yes. I love them. The Oil Based ones. I made 35 Red Cardinals and offered people personal names on them. They came out beautifully. I used the extra fine point
Re: Sharpie paint pens
Posted: Wed Dec 17, 2014 3:20 pm
by Georgia Novak
How high did you fire the paint from the pens?
Re: Sharpie paint pens
Posted: Wed Dec 17, 2014 11:15 pm
by vblue
I tried the silver and gold pens. The gold turned dark but the silver was okay. I took it to around 1500. Have you tried any other colors?
Re: Sharpie paint pens
Posted: Fri Dec 19, 2014 1:19 pm
by Aglassygirl303
I used the gold after I fired the piece
Re: Sharpie paint pens
Posted: Fri Dec 19, 2014 1:19 pm
by Aglassygirl303
I used the gold after I fired the piece