I have a stainless steel bowl with no lip at the
top, just a small edge that is the thickness
of the steel. Can my glass that I will slump into this
mold hang over the rim/lip? 1/2" to 3/4" inches outside?
I learned a few days back this will not work
on a ceramoc drop through.
Thanks
BZody
Tony Serviente
Posts: 328
Joined: Thu May 29, 2003 11:48 am
Location: Ithaca,NY
Contact:

Post by Tony Serviente »

Depends on how smooth the edge is. If it is a nice rolled edge, and not a rough saw cut , I am guessing it will work. Other factors are the height and diameter of the form, but if the edge is smooth I think it will work. Just don't forget to kiln wash it.
Bryan
Posts: 26
Joined: Wed Jan 07, 2004 4:42 pm
Location: Houston,TX

Post by Bryan »

It is a saw cut, but has been ground smooth.