Ceramic kilns for fusing glass in schools
Posted: Fri Mar 27, 2015 11:25 pm
I'm teaching another Intro. To Glass Fusing class to FWISD Art Teachers. These are teachers who have never even cut glass. Half of the teachers in this class are elementary teachers who have ceramic kilns.
Most of the teachers that I have taught in the past have new kilns that fire glass. This is the first class I've had with this many with ceramic kilns.
I have never used a ceramic kiln. I know the difference in element placement, etc. I need something to help guide them in firing their kilns for glass. I found one item on Paragon's website.
Anyone have any resources, info. site for videos, etc. that can help them?
Any help will be greatly appreciated.
Vernelle
Most of the teachers that I have taught in the past have new kilns that fire glass. This is the first class I've had with this many with ceramic kilns.
I have never used a ceramic kiln. I know the difference in element placement, etc. I need something to help guide them in firing their kilns for glass. I found one item on Paragon's website.
Anyone have any resources, info. site for videos, etc. that can help them?
Any help will be greatly appreciated.
Vernelle