Postby Kathy K » Sat Oct 10, 2015 3:25 pm

A friend of mine had been given several glass power tools from someone else and she wanted them out of her shop so I purchased very inexpensively. One of the things that I ended up with is, I believe, a Covington wet belt sander. Am not finding the equivalent online so assume it is a bit older. It needs some TLC, cleanup, etc. Has a little chipping pain and a small amount of rust, however it runs well and quietly. Any idea what model and where I can buy parts....will have my better half work on refurbing it a bit, but he likes me to find the parts. It doesn't have a model number but does say Covington, as well as Nervo Distributors in Berkley, CA. Looks a bit like the Covington with the Muslin Buff Polisher but seems like it has an extra wheel.
Any info you might have would be very helpful. Picture attached.
thanks,
Kathy
Attachments
DSC00186.JPG
DSC00184.JPG

Brad Walker
Site Admin
Posts: 1335
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Covington Wet belt sander?

Postby Brad Walker » Sat Oct 10, 2015 3:57 pm

Contact Covington: http://covington-engineering.com/

They've made dozens of different models, some as one offs, but should have parts and advice for one and all.

Bert Weiss
Posts: 2337
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Covington Wet belt sander?

Postby Bert Weiss » Sat Oct 10, 2015 9:51 pm

You use a sponge for the water delivery on this. I buy wet belts from CR Laurence. You need an account. I am sure there are many sources for 3 x 24 carbide wet belts.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions

Buttercup
Posts: 552
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Covington Wet belt sander?

Postby Buttercup » Mon Oct 12, 2015 3:05 am

Not trusting the sponge I rigged up a plastic container with a drip line that gravity feeds to the belt. One day I'll get lockline to make positioning of the drip line a bit more accurate. Jen

Edit: Pictures hadn't shown when I responded. Mine is a later model but I'd still be inclined to use a gravity water feed on yours. (Nice bonus outrigger!)
Last edited by Buttercup on Wed Oct 14, 2015 5:28 pm, edited 1 time in total.

Kathy K
Posts: 36
Joined: Fri Jun 01, 2007 9:29 pm
Location: Gresham, OR

Re: Covington Wet belt sander?

Postby Kathy K » Wed Oct 14, 2015 10:33 am

Thanks for your help. I have emailed Covington and not heard back from them.
Hoping I can at least get the belt sander up and running.

Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: Covington Wet belt sander?

Postby Valerie Adams » Wed Oct 14, 2015 12:38 pm

I think I've got belts that would fit that! I purchased from someone else, thinking they'd fit mine but they're much too small. Message me if you're interested and I'll measure them.

Kathy K
Posts: 36
Joined: Fri Jun 01, 2007 9:29 pm
Location: Gresham, OR

Re: Covington Wet belt sander?

Postby Kathy K » Mon Oct 26, 2015 12:29 pm

Hi Valerie,
Sent a PM and an email. Would love to discuss your sanding belts.
thanks,
Kathy

Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: Covington Wet belt sander?

Postby Valerie Adams » Tue Oct 27, 2015 1:03 am

Finally saw your message and have sent you two PMs :oops:

Kathy K
Posts: 36
Joined: Fri Jun 01, 2007 9:29 pm
Location: Gresham, OR

Re: Covington Wet belt sander?

Postby Kathy K » Tue Oct 27, 2015 1:18 pm

Hi Valerie,
I have sent you a PM in return.
Thanks,
Kathy


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 39 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com