Vermiculite Board
Posted: Thu Jun 23, 2016 4:28 pm
I am building a small kiln (a cubic ft.) --- I've seen different boards mentioned to line the kiln with.
Delphi Glass has a Vermiculite Board (their number 92807) --- is this something that will work for the inside liner?
The outside will be IFB's.
I have ceramic blanket left over from our hot glass/batch days --- but I thought some kind of board would be easier
to work with on the walls.
Thanks,
Terry