Hello ! Please can anybody give me a schedule for firing and slumping a bowl of Car window Glass (I hope I use the right words in English for this material :) ) Thank you, Jan from Holland

Re: Car window glass

Posted: Wed Apr 26, 2017 4:38 pm
by DonMcClennen
Car window glass use to be 2 thin layers of a glass sandwich with a thin plastic layer in the middle. If this is still the way its made then fusing is not an option..

Re: Car window glass

Posted: Thu Apr 27, 2017 11:22 am
by Rick Wilton
Car WINDOWS are tempered....... car windshields are laminated.

Windows good to fuse

Windshields NOPE

Re: Car window glass

Posted: Fri May 12, 2017 5:47 am
by Jan de Jong
Rick Wilton wrote:Car WINDOWS are tempered....... car windshields are laminated.

Windows good to fuse

Windshields NOPE
Thank you for your answer and sorry for the late response (waiting on a mail that there was a post, but that was in the paste !) But do you have a schedule for fusing and slumping this glass (or is that the same as "normal" window glass) ?? Jan de Jong (from Holland)