healing a broken piece of glas.

Posted: Fri May 05, 2017 9:46 pm
by jim simmons
I would like to know how to eliminate/minimize a break.
I have a piece of BE that broke and I still want to use to make a bowl.
Should the break be put on the top or the bottom of the 2 layer stack for the fusing?
Thanks
The other Jim

Re: healing a broken piece of glas.

Posted: Sat May 06, 2017 9:31 am
by The Hobbyist
The bottom.

Jim "The Hobbyist"