Hello ! Is there a simple way to make a "rainbow" (half-circle) with 6-7 colours ? Jan de Jong
Re: Making a rainbow
Posted: Fri Jun 30, 2017 3:58 pm
by jim simmons
Sure.
cut a circle then cut it in half and layer different frits on it.
The other Jim
Re: Making a rainbow
Posted: Sun Jul 02, 2017 4:47 am
by Jan de Jong
jim simmons wrote:Sure.
cut a circle then cut it in half and layer different frits on it.
The other Jim
Thank you Jim ! Is there a way to do it with sheet glass (as I still did not work with frits and not have them). Is it possible with a saw ? Jan
Re: Making a rainbow
Posted: Sun Jul 02, 2017 7:29 am
by Fiona Collins
Cut a half sheet of clear and butt against 1/2 sheet of first colour. Place your circle cutter in the middle of the join, score half circle on the colour sheet, adust length in 15mm, leave base as is, run second score. Replace colour sheet with second colour, score with same setting as previous, adjust length in 15mm ... rinse and repeat 4 times. Carefully run and break out each segment
Re: Making a rainbow
Posted: Wed Jul 05, 2017 5:00 am
by Jan de Jong
@ Fiona Collins: Thank you ! Jan