fill weight and firing schedule?
Posted: Wed Oct 25, 2017 12:18 am
Does anyone have a fill weight for each cast heart and a firing schedule for this casting mold?
Guide to fusing, slumping, and related kilnforming techniques
https://warmglass.com/phpBB3/
Alternatively, just fill the mold and fire. Weigh the finished piece. If it's too big, subtract some frit next time. If it's too small, add some frit.Peter McCarthy wrote:Glass weighs 2.5 times as much as water. Weigh the amount of water that fills a heart and multiply by 2.5 for the amount of glass needed.