Glass blowing is the most interesting art form for me. I was thinking to overcome of hard logistics of glass blowing shop, I thought , it would be interesting to blow cold or warm semi liquid , semi set polymer.
We blow glass because it sets slowly.
Thermoset plastics can be engineered to lose their liquid form in desired way with chemical engineering. They comes in two parts , resin and hardener and higher the hardemner mix , lower the set time.
Now there are immense amount of polymers and there are immense amount of polymer engineering firms. There are polymers more transparent than glass.
Lets talk about facts . How we describe , which properties describe the molten blowing glass. What makes it ? What we will research similar in plastics to
molten glass.
Thank you,
Mustafa Umut Sarac
Istanbul
Re: Which properties makes blowing glass ? Engineering Cold Warm Thermoset Polymer Glass Blowing
Posted: Fri Feb 23, 2018 12:47 pm
by Brad Walker
Most of the people who frequent this website are interested in kilnformed glass, not blown glass.
A good forum for glassblowing discussion is located at:
http://talk.craftweb.com/forumdisplay.php?s=&forumid=4
Re: Which properties makes blowing glass ? Engineering Cold Warm Thermoset Polymer Glass Blowing
Posted: Fri Feb 23, 2018 1:02 pm
by Mustafa Umut Sarac
they dont accept gmail and i dont accept their rule.
Re: Which properties makes blowing glass ? Engineering Cold Warm Thermoset Polymer Glass Blowing
Posted: Fri Feb 23, 2018 1:16 pm
by Brad Walker
Mustafa Umut Sarac wrote:they dont accept gmail and i dont accept their rule.
Then I guess you can't get their help either.
Re: Which properties makes blowing glass ? Engineering Cold Warm Thermoset Polymer Glass Blowing
Posted: Fri Feb 23, 2018 1:35 pm
by Mustafa Umut Sarac
someone will discuss here.If you dont , dont pirate the thread.
Re: Which properties makes blowing glass ? Engineering Cold Warm Thermoset Polymer Glass Blowing
Posted: Sun Feb 25, 2018 9:40 pm
by Marty
We haven't had acrimony on this board for a long time- I'm not sure whether I'd rather see inactivity or conflict.
Mustafa- This board is not the place you're looking for, and I don't think you'd get far on craftweb either. As Brad (the owner of this board) said, we're mostly interested in fusing glass. On Craftweb they don't want to blow plastic and I'd think that most of them are not all that interested in discussing the physics and chemistry of glass unless it pertains to immediate issues, not blue sky speculation.
You might try asking the librarians at the Rakow Library in Corning to see if they can point you in a useful direction.
Please be polite to them, they're the most kind, wonderful people.
Marty
Re: Which properties makes blowing glass ? Engineering Cold Warm Thermoset Polymer Glass Blowing
Posted: Sun Feb 25, 2018 10:21 pm
by Buttercup
Excellent advice, Marty.......was trying to think how best to frame advice around a topic I know little about.