firing schedule
Posted: Fri Jul 20, 2018 3:29 pm
mine: for three layer 71/2 x 11 assembled frit sheets. which works
300 1215 2.00
100 1490 :20
9999 910 2:00
100 750 .15
However I am now doing four layers of 12x12 assembled frit sheets. Do you think I need to change this schedule at all. Thank you for any advice, I'm really bad at changing schedules that I know work.
300 1215 2.00
100 1490 :20
9999 910 2:00
100 750 .15
However I am now doing four layers of 12x12 assembled frit sheets. Do you think I need to change this schedule at all. Thank you for any advice, I'm really bad at changing schedules that I know work.