Those of you in the know, does this System 96 glass color strike? If this is the orange I think it is, it color shifts to orange/ brown at fusing temps.
#96-675.5G Godiva
Does this Color Strike?
Moderators: Brad Walker, Tony Smith
Re: Does this Color Strike?
The pic didn't attach. Sorry.
Nor did it again. Well, the color is easily Google-able. So sorry.
Nor did it again. Well, the color is easily Google-able. So sorry.
-
Brad Walker
- Site Admin
- Posts: 1540
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Does this Color Strike?
Probably strikes, most oranges/reds do.