Is it possible to make a small bowl in a kiln washed mold by pressing glass powder "paste" into the inside surface and tack firing? It seems reasonable as that is a method used for making the "ice bowls" from tempered glass bits. There must be some cosmic force thing I don't recognize that dictates the use of a break away mold. I'm not trying for anything other than a simple little bowl.
Thanks
Vonon
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: pate de verre-ish

Post by Kevin Midgley »

watch your temperatures LOL

Look through the files on Warmglass
Like this in the photo section.
http://www.warmglass.com/phpBB3/viewtop ... re#p351974
Vonon
Posts: 195
Joined: Fri Mar 10, 2006 6:32 pm
Location: East Tennessee

Re: pate de verre-ish

Post by Vonon »

Thanks Kevin. I assume you're cautioning me to keep the temp. low enough to avoid a puddle at the bottom of the pot. I enjoyed revisiting the posts in the archives and was amused to find one of my own in that group.
Vonon
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: pate de verre-ish

Post by Kevin Midgley »

Or you need to pack an inner shell holding the carefully placed powder in place.