Has anyone tried doing a pot melt onto fiber paper or Thin Fire?

Thanks
Michael
charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Post by charlie »

yes. don't. it will pull up fibers or dust into the glass, cause ugliness at the best, and incompatibilities and cracking at the worst.

i use a piece of glass for the melt to land on, and very fine layer of baby talc under that to allow the glass to slide without sticking.
Tyler Frisby
Posts: 75
Joined: Tue Dec 02, 2003 8:27 pm
Location: Canada

Post by Tyler Frisby »

Any problems trying a Pot melt into a plaster/silica mold ? Ive thought It would be really swank to try :) tanks a Milly