Vanilla (sulfur) and Coral Sunset (lead) for 96 COE!

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
danieljanse
Posts: 9
Joined: Sat Feb 02, 2019 5:37 pm

Vanilla (sulfur) and Coral Sunset (lead) for 96 COE!

Post by danieljanse »

Hi. I'm trying to recreate this reaction in 96COE. I tried this a long time ago with a glass color called Ivory. I now think that this color did not contain sulfur/selenium so I was doomed from the start! So, Oceanside is making a Vanilla that is reactive like Bullseye and I'm going to try again. But, what 96 COE color can I count on to provide the lead? From what I can tell, Oceanside is avoiding the use of lead. If anyone has been able to achieve this reaction in 96COE I'd appreciate some guidance. Thanks!