Page 1 of 1

Mother of Pearl Powders

Posted: Fri Apr 09, 2004 3:27 pm
by nbaybear
Has anyone used Mother of Pearl powders with either COE 96 or 90, would like to try but not sure if they are compatable


Thanks Randy :lol:

Re: Mother of Pearl Powders

Posted: Fri Apr 09, 2004 3:36 pm
by Brock
nbaybear wrote:Has anyone used Mother of Pearl powders with either COE 96 or 90, would like to try but not sure if they are compatable


Thanks Randy :lol:
Compatability won't be a problem, but what is this stuff? If it's real nacre, it's just gonna burn up. Maybe they're another form of mica? Brock

Posted: Fri Apr 09, 2004 6:14 pm
by Ron Coleman
If the Mother of Pearl powders are the ones from CR Loo, they will work.

Just another name for mica powders.