Page 1 of 1
Black Pipe Pattern Bars
Posted: Sun Apr 11, 2004 4:41 pm
by Judy Schnabel
Just finished a panel using techniques described by Kevin O'Toole in Glass Craftsman magazine.
No critique necessary. Just sharing what I thought was fun to create.
http://www.picturetrail.com/gallery/vie ... &members=1
flower garden
Posted: Sun Apr 11, 2004 7:20 pm
by Ann Demko
Judy, Your flower garden does look like fun. I tried the fusing in a lead pipe and it came out well but there are some grayish spots in the glass. I don't know if it is some lead filings that I didn't get out with my magnets when I made frit or if it was stuff that flaked off the sides of the pipe. Did you have any inclusions in your pieces? Ann
Posted: Sun Apr 11, 2004 7:26 pm
by Judy Schnabel
Ann,
I lined the pipe with fiber paper and just filled the pipes with strips of glass. Next time I'll put more clear in the pipes. I didn't have anything flake off the pipes onto the glass though.
Like I said, it was fun. Plus, I belong to our local sculptor's group and they are always pushing us for new work for when we're called upon to do an exhibition.
I used 1 1/2" pipe for this one but I'm going back and get some 2" pipe so all the "flowers" won't be the same size.
Judy
Posted: Sun Apr 18, 2004 1:58 pm
by Mitcheal
I don't think I've seen this article? Is it in the current magazine? or a previous one, I dropped my subscription last year, but have recently renewed it...
Mitcheal
Posted: Sun Apr 18, 2004 3:42 pm
by Judy Schnabel
I believe it was around November of 2003. In that particular issue it did not have a month on the front.
Judy
Posted: Mon Apr 19, 2004 4:33 pm
by Mitcheal
Thanks, I'll have to look for that issue.. I don't currently posses a copy of it.
Thanks again for the info.