Cleaning kiln shelves (fabricut)

Post by Jon Wunderlich »

I know there have been many discussions on this subject before but I've been using Fabricut for a couple of weeks to clean kiln wash off my shelf and I just love this stuff. Quick and easy, wash it out after, and it's cheap too. I got it at A&A products, (didn't see it offered by any of the board sponsors, but I may have missed that). Does anyone else use this?

Jon
Mike Byers
Posts: 56
Joined: Mon Mar 10, 2003 6:57 pm
Location: west central Indiana
Contact:

Post by Mike Byers »

I use the open-weave stuff (similar to Fabricut) that's used to sand drywall, but only to clean up any remaining kilnwash after I've scraped it off. An 8" drywall taping knife makes a good scraper: just a few passes and the shelf is mostly cleaned off. Very little dust, too.