Search found 8 matches
- Thu Apr 03, 2014 5:28 am
- Forum: Photos and Stuff
- Topic: Blankets X 2
- Replies: 15
- Views: 42252
Re: Blankets X 2
I just love your work. I have liked your page on Facebook.
- Sat Mar 15, 2014 1:23 am
- Forum: Newcomer Forum
- Topic: Red splotchy contamination on lemon grass colour
- Replies: 6
- Views: 27900
Re: Red splotchy contamination on lemon grass colour
Thanks Cynthia, everyday is a new learning day!
- Fri Mar 14, 2014 10:21 pm
- Forum: Newcomer Forum
- Topic: Red splotchy contamination on lemon grass colour
- Replies: 6
- Views: 27900
Re: Red splotchy contamination on lemon grass colour
Thanks Dana, I would imagine that is the problem. Do you know any way to mix those colours without having the contamination problem?
- Fri Mar 14, 2014 7:44 pm
- Forum: Newcomer Forum
- Topic: Red splotchy contamination on lemon grass colour
- Replies: 6
- Views: 27900
Re: Red splotchy contamination on lemon grass colour
If the nearest bullseye distributor wasn't 1000 kilometres away, I probably would use it.
- Fri Mar 14, 2014 6:57 pm
- Forum: Newcomer Forum
- Topic: Red splotchy contamination on lemon grass colour
- Replies: 6
- Views: 27900
Red splotchy contamination on lemon grass colour
image.jpg Hi Everyone, I have attached a rather grainy photo to show the problems I'm having problems with a spectrum glass colour lemon grass. When it went into the kiln to slump, it was fine, when it came out of the kiln, only the lemon had the red colour splotchy contamination. It is only on the...
- Fri Jun 07, 2013 1:50 am
- Forum: Newcomer Forum
- Topic: Thermal shock or careless handling?
- Replies: 16
- Views: 38104
Re: Thermal shock or careless handling?
Thanks Bert, will adjust my schedule accordingly. You've mentioned the Stone book a few times, think I might finally purchase one.
- Thu Jun 06, 2013 9:05 pm
- Forum: Newcomer Forum
- Topic: Thermal shock or careless handling?
- Replies: 16
- Views: 38104
Re: Thermal shock or careless handling?
Thanks for all your very helpful answers, I really appreciate the time everyone has taken to reply. I will convert the Celsius to Fahrenheit so it makes it easier to read. I will try to include all the extra information that you have asked for. I guess I have a whole lot of things going wrong with m...
- Thu Jun 06, 2013 6:01 am
- Forum: Newcomer Forum
- Topic: Thermal shock or careless handling?
- Replies: 16
- Views: 38104
Thermal shock or careless handling?
Hi Everyone, I have been reading this forum for quite a while now and have found it extremely informative. Now I need to put my problem out there and see what everyone thinks. I have been making bowls using a strip construction technique for about a year. I use System 96. I have my work in various g...