Search found 3 matches

by Laurie Schock
Mon Feb 10, 2014 1:09 pm
Forum: Techniques and Tools
Topic: Wax Vac, no its not what you think!
Replies: 12
Views: 25698

Re: Wax Vac, no its not what you think!

Is that the goofy ear wax thing???
by Laurie Schock
Fri Jan 10, 2014 4:53 pm
Forum: Techniques and Tools
Topic: Glue for fused work
Replies: 24
Views: 66153

Re: Glue for fused work

Havi-i use the aloe vera gel as a glue.... Water it down and you can either spray it, brush it or apply it to the glass to hold whatever it is you need held. I haven't had any devit, discoloration or problems using it.
by Laurie Schock
Mon Jan 06, 2014 11:50 am
Forum: Techniques and Tools
Topic: Glue for fused work
Replies: 24
Views: 66153

Re: Glue for fused work

Have you tried cheap aloe vera gel? Water it down to the consistency that works for you.... It works great!