Search found 2 matches
- Tue Jul 15, 2003 2:32 pm
- Forum: Kiln Casting
- Topic: Pâte de verre casts
- Replies: 2
- Views: 6611
Pâte de verre casts
My name is Jianu Vladimir and I am a Romanian artist working in pâte de verre. I face some problems that I have been trying to solve on my own for about one year now but with no significant progress and I hope that someone more experienced than me might help me. My most important problem is that th...
- Fri Jul 11, 2003 2:32 pm
- Forum: Techniques and Tools
- Topic: Pâte de verre
- Replies: 2
- Views: 5874
Pâte de verre
My name is Jianu Vladimir and I am a Romanian artist working in pâte de verre. I face some problems that I have been trying to solve on my own for about one year now but with no significant progress and I hope that someone more experienced than me might help me. My most important problem is that th...