Search found 7 matches

by grayeye
Tue May 06, 2014 7:16 pm
Forum: Jewelry Making
Topic: ramping schedule
Replies: 6
Views: 35660

Re: ramping schedule

there were instructions, but it didn't turn out. I don't want to test fire the ones I got from AAE until I have some sort of ramping schedule for my kiln. I bought it used. I have figured out one for firing my glass but now I would like to move on to decals. I only have an infinity switch on there s...
by grayeye
Tue Apr 29, 2014 3:10 pm
Forum: Newcomer Forum
Topic: Orange park/ Jacksonville Florida
Replies: 4
Views: 8012

Re: Orange park/ Jacksonville Florida

for anyone else who may have had the same question, I did find a place in St. Augustine that has a little bit of coe 90 and 96. the shop is small but the owners are very friendly and helpful and will try to order just about anything you ask for. The name of the shop is D & L glass. they deal in ...
by grayeye
Tue Apr 29, 2014 2:55 pm
Forum: Jewelry Making
Topic: ramping schedule
Replies: 6
Views: 35660

ramping schedule

can anyone give me a ramping schedule for high fire and low fire decals? I don't want to sacrifice any more decals...
I have a Vulcan 111f
by grayeye
Thu Mar 20, 2014 7:34 pm
Forum: Newcomer Forum
Topic: Orange park/ Jacksonville Florida
Replies: 4
Views: 8012

Re: Orange park/ Jacksonville Florida

okay
Thank you.
by grayeye
Sat Mar 15, 2014 9:23 pm
Forum: Jewelry Making
Topic: okay so I got the shape I want with the grinder but now..
Replies: 3
Views: 29569

Re: okay so I got the shape I want with the grinder but now.

Thank you.
What is firepolish? and how do I do it?
by grayeye
Sat Mar 15, 2014 9:21 pm
Forum: Newcomer Forum
Topic: Orange park/ Jacksonville Florida
Replies: 4
Views: 8012

Orange park/ Jacksonville Florida

Is anyone in this area that could tell me where I can get 90 coe glass locally? I realize I can go online but I really like to see what I'm buying in person and when I really want something online there seems to be either a huge minimum purchase or exorbitant shipping fees. Are there any glass facto...
by grayeye
Sat Mar 15, 2014 5:33 pm
Forum: Jewelry Making
Topic: okay so I got the shape I want with the grinder but now..
Replies: 3
Views: 29569

okay so I got the shape I want with the grinder but now..

I used a glass grinder to shape the pieces because they looked like blobs (after using a microwave kiln) but now the edges are ugly mat black. now what?