Search found 2 matches

by Vicky Harris
Sun Jan 04, 2015 2:44 am
Forum: Newcomer Forum
Topic: Slumping disaster - HELP!
Replies: 4
Views: 13160

Re: Slumping disaster - HELP!

Thanks for your comments. Yes I have 4 coats of kiln wash on the molds and the design is really good/clear on the glass. Should I try more kiln wash and lower top temp? If I full fuse the bowl do you think it'll go round and flat or am I going to end up with another problem?

Thanks, Vicky
by Vicky Harris
Sat Jan 03, 2015 9:43 pm
Forum: Newcomer Forum
Topic: Slumping disaster - HELP!
Replies: 4
Views: 13160

Slumping disaster - HELP!

I am making a rainbow dinner set and am to the slumping stage. The dinner plates and side plates have come out great, but two bowls I did yesterday have got rough top edges (https://www.dropbox.com/s/tsja1cmevmw42l2/darkbluebowl.jpg?dl=0). They are going into Slumpys molds and I used the Slumpys rec...