Re: How to make perfect oval cabochons like from Etsy
Hi Jenna, thank you very much for your answer. I am refering to the perfectly uniform clear oval cabochons from Etsy. Yes, I know about the doming, however, I'd be grateful if I could get a little less of it.. So far, I found out you can buy a glass cutting machine, cut ovals and "fire polish&q...
- Fri Jan 09, 2015 1:42 pm
- Forum: Jewelry Making
- Topic: How to make perfect oval cabochons like from Etsy
- Replies: 4
- Views: 34317
How to make perfect oval cabochons like from Etsy
Hello, I'm a newbie in jewelry making and glass fusing. I've been playing around with some of the 30x40mm oval cabochons from Etsy but I don't like the domed shape. I'd like to make my owns, but I don't get anywhere close to them :( If I cut a diamond shape, I can't control how the glass flows too w...