Search found 2 matches

by michelle andre
Thu Nov 06, 2003 1:54 pm
Forum: Techniques and Tools
Topic: vermiculite board
Replies: 5
Views: 12971

vermiculite board

Does anyone know where I can get vermiculite board? I use it to make various slumping molds. It is great to work with because it cuts easily, it allows the glass to breathe,and is reusable. I used to purchase it from Seattle Pottery but I have had shipping woes and problems with customer service tim...
by michelle andre
Fri Jul 18, 2003 10:35 am
Forum: Techniques and Tools
Topic: Cutting pattern bars
Replies: 3
Views: 10052

Cutting pattern bars

I have been trying to cut a pattern bar ( approx. 1"x1") with a tile saw that has a 8" diamond wheel. The cut seems to go well until the last bit where a chunk of the the bar breaks off and leaves a nub on the pattern tile I have just cut. Does anyone have any suggestions on how I mig...