How to prepare fiber paper?
Hi, I just ordered some fiber paper and have a question about firing it for use. I know the tutorial says to vent the kiln. Does this mean that all I need to do is crack the kiln door while firing it up? Do I wait until the kiln reaches a certain temp before venting, or should the door be open a bit...