Search found 8 matches

by Higgins Glass
Mon Feb 16, 2004 2:32 pm
Forum: Techniques and Tools
Topic: Frances Stewart Higgins 1912 - 2004
Replies: 4
Views: 10600

Frances Stewart Higgins 1912 - 2004

I am sorry to inform you that noted glass artist Frances Higgins died 2-12-04 at her Home/Studio in Riverside , IL. This Pioneer of fusing will be missed deeply.
Please read more at our website http://www.higginsglass.com .

Thank You, from everyone at the Higgins Glass Studio.
by Higgins Glass
Fri Jan 09, 2004 12:57 pm
Forum: Techniques and Tools
Topic: Plug for the Site
Replies: 1
Views: 6033

Plug for the Site

Hi all, I am just writing to say at the end of December the Studio was filmed for an upcoming piece on Art Beat Chicago that airs on channel 11. We think it will air sometime at the end of January, will keep you updated. The host (Fawn Ring) ask about places to get more information about Fusing and ...
by Higgins Glass
Tue Oct 21, 2003 2:34 pm
Forum: Techniques and Tools
Topic: Drop Ring Material
Replies: 3
Views: 9142

Hi,
I agree with Tom making your own ceramic clay Drop Out molds is the way to go. That is what we do and it's not that hard, also they last a long time, we have some from the 60's we still use.
Have fun!
Jon
by Higgins Glass
Tue Jul 29, 2003 2:56 pm
Forum: Techniques and Tools
Topic: First Post From Higgins Glass
Replies: 17
Views: 34702

Sorry I have not been able to reply, Very busy lately. I will say Thank You for your great response!!! I will get to your questions soon but for now I just posted some Pieces on Ebay and I thought you might like to take a look. Talk To All Of You Soon!! Thanks, Jon http://cgi6.ebay.com/ws/eBayISAPI....
by Higgins Glass
Wed Jul 23, 2003 4:36 pm
Forum: Techniques and Tools
Topic: First Post From Higgins Glass
Replies: 17
Views: 34702

Your welcome Brock it was my pleasure, I'm glad you are sharing Frances and Michaels story with everyone. I'm sure we will be talking more.

Jon
by Higgins Glass
Wed Jul 23, 2003 4:10 pm
Forum: Techniques and Tools
Topic: First Post From Higgins Glass
Replies: 17
Views: 34702

Hi, It is very inspiring Tony, to say the least. I am not blood related ( Frances and Michael never had children) but I am as close as it gets , they have always been like my Grandparents. I have been making my own pieces for many years now and hope to post some photos soon ( if I can only figure ou...
by Higgins Glass
Wed Jul 23, 2003 3:16 pm
Forum: Techniques and Tools
Topic: First Post From Higgins Glass
Replies: 17
Views: 34702

First Post From Higgins Glass

Hi, My name is Jon and I work for the Higgins Glass Studio in Riverside, IL. I have been working for the Higgins Studio for over 12 years (but grew up in the Studio from the age of two)and love it. I look forward from hearing from all of you and I hope I can Help in anyway. Thanks, Jon P.S. Frances ...
by Higgins Glass
Wed Jul 23, 2003 2:07 pm
Forum: Techniques and Tools
Topic: UV Light
Replies: 11
Views: 22669

Hi, In my experience at our Studio the Tin does effect cretin colors, making them look duller then normal, because of this we avoid the Tin at all cost. I do agree with Tony that it is something you will have to decide for yourself because everyone has there own style and what works for one person d...