Re: MR-97 application problems

I just want to tell everyone about a very impressive experience I had; I had been having problems when spraying MR-97 on a molds the spray was not leaving a smooth texture on the molds it had a sand like texture; I had posed question on every glass fusing web site I could find and no one had an answ...
by mtn gator
Tue Oct 06, 2015 3:05 pm
Forum: Newcomer Forum
Topic: MR-97 application problems
Replies: 0
Views: 4127

MR-97 application problems

I just want to tell everyone about a very impressive experience I had; I had been having problems when spraying MR-97 on a molds the spray was not leaving a smooth texture on the molds it had a sand like texture; I had posed question on every glass fusing web site I could find and no one had an answ...
by mtn gator
Tue Sep 29, 2015 12:52 pm
Forum: Newcomer Forum
Topic: MR-97 application problems
Replies: 6
Views: 8716

MR-97 application problems

I'm having an application problem with MR-97, when I spray molds the MR-97 has a rough texture like fine sand. I am following all of the instructions I shake the can well before using, I hold the can vertical not at an angle, I'm making sure the mold is 10-12 inches away and it doesn't matter if the...