Search found 4 matches

by Renee Inman
Sun Jan 10, 2016 12:54 pm
Forum: Newcomer Forum
Topic: Delphi Mold Disaster- Suggestions please :)
Replies: 7
Views: 30706

Re: Delphi Mold Disaster- Suggestions please :)

Many thanks to everyone who contributed here! You've shortened my learning curve tremendously!
by Renee Inman
Sat Jan 02, 2016 2:30 pm
Forum: Newcomer Forum
Topic: Delphi Mold Disaster- Suggestions please :)
Replies: 7
Views: 30706

Re: Delphi Mold Disaster- Suggestions please :)

Yes, I used two pieces of sheet glass. That's part of what made the outcome so surprising. Any other thoughts/suggestions?
by Renee Inman
Fri Jan 01, 2016 1:44 pm
Forum: Newcomer Forum
Topic: Delphi Mold Disaster- Suggestions please :)
Replies: 7
Views: 30706

Delphi Mold Disaster- Suggestions please :)

I've included a photo of my disaster and the instructions/firing schedule I used. I did not use an impression on my project. Followed Delphi's firing schedule and used 90 COE glass throughout. My plate ended up with "holes" in 3 out of 4 corners. Next time I use this mold I will try: Check...
by Renee Inman
Fri Jan 01, 2016 1:05 pm
Forum: Newcomer Forum
Topic: impression tile and rimmed dish mold
Replies: 4
Views: 19640

Re: impression tile and rimmed dish mold

I'm also interested in any insights shared here. I used the same mold, but without an impression. Followed Delphi's firing schedule and used 90 COE glass throughout. My plate ended up with "holes" in 3 out of 4 corners. Next time I use this mold I will Check to make sure mold holes are cle...