Search found 2 matches
- Tue Dec 06, 2016 1:31 am
- Forum: Newcomer Forum
- Topic: Casting in vacuum furnace
- Replies: 1
- Views: 5622
Casting in vacuum furnace
I have a vacuum furnace I can set up. I want to cast glass into a mold. The unit is rated for 1100c. If the glass will slump I'm guessing without air it may conform to a mold. The question is, Is this possible at all at 1100c? What would be the lowest temperature without air/bubble worry? I need to ...
- Mon Dec 05, 2016 1:12 pm
- Forum: Kiln Casting
- Topic: is casting ar 1100c possible
- Replies: 1
- Views: 6747
is casting ar 1100c possible
I have a vacuum furnace I can set up. I need some electrical work for it. I want to cast glass into a mold. The unit is rated for 1100c. If the glass will slump I'm guessing without air it may conform to a mold. The question is, Is this possible at all at 1100c?