Search found 3 matches

by clenzly
Fri Feb 05, 2021 12:36 am
Forum: Techniques and Tools
Topic: Wave Mold Slump Breakage
Replies: 5
Views: 36769

Re: Wave Mold Slump Breakage

I will try the slower ramp uo
by clenzly
Fri Feb 05, 2021 12:11 am
Forum: Techniques and Tools
Topic: Wave Mold Slump Breakage
Replies: 5
Views: 36769

Re: Wave Mold Slump Breakage

I’m using Bullseye glass. The top portion is one layer. The bottom portion is 2 layers with 2 layers of fiber paper used to make the pockets. I don’t have an issue when I create the pockets. Just when I try to slump. The issue seems to be where the single layer meets the double layer. That’s normall...
by clenzly
Tue Jan 12, 2021 5:50 pm
Forum: Techniques and Tools
Topic: Wave Mold Slump Breakage
Replies: 5
Views: 36769

Wave Mold Slump Breakage

I have been attempting to slump a pocket vase using a wave mold. The initial mold to create the pocket works fine. However, almost every attempt to slump it using the wave mold breaks. I've tried several schedules and have been unsuccessful. Do you guys have any ideas that might help me? The last sc...