Topic: Help! Can my ceramic frit mold be saved?
Replies: 2
Views: 159190

Help! Can my ceramic frit mold be saved?

I have been screwing up my attempts at kiln casting and am afraid I am destroying my molds in the process. My glass is sticking in spite of applications of ZYP, forcing me to fire them again upside down to try to remove the stuck glass. I got most of it out, but as you can see, some has remained on ...
by Sue Bell
Thu Jul 11, 2019 3:13 pm
Forum: Newcomer Forum
Topic: Novice looking for help with Fuseworks Craft kiln
Replies: 1
Views: 11484

Novice looking for help with Fuseworks Craft kiln

I am a novice and pretty much self taught with no convenient access to classes other than via the internet. I play with glass mosaics and fused glass using the Fuseworks microwave kiln and the new Fuseworks Craft kiln. I am hoping that there might be others on this message board who have experience ...