Search found 8 matches
- Fri Aug 02, 2024 4:46 pm
- Forum: Techniques and Tools
- Topic: Amaco Glass
- Replies: 1
- Views: 40828
Amaco Glass
Has anyone used Amaco glass? I found several sample boxes, its all marked COE 90. I use 96. I've done a few firings with the Amaco using a schedule that works for 96 (not mixing the 90 and 96) and so far so good. I suspect this stuff is old.
- Wed Nov 30, 2022 2:46 pm
- Forum: Techniques and Tools
- Topic: reflective backing?
- Replies: 4
- Views: 11192
Re: reflective backing?
If the adhesive will stick to a painted surface it might be OK. But if the adhesive instructions say to remove any paint, then it probably won't work.
- Wed Nov 30, 2022 6:33 am
- Forum: Techniques and Tools
- Topic: reflective backing?
- Replies: 4
- Views: 11192
Re: reflective backing?
Rust-Oleum makes a spray paint for this. It gets applied to the back, after firing. Also needs a clear coat after the reflective finish is applied. Read and follow the directions. It doesn't give a mirror-like finish but it does reflect. It also seems to highlight every little imperfection in the gl...
- Wed Sep 14, 2022 3:50 pm
- Forum: Techniques and Tools
- Topic: Bubble
- Replies: 2
- Views: 9505
Re: Bubble
I think I found the answer ... right here on this website. I'll try adjusting my schedule.
https://warmglass.com/what-caused-this-huge-bubble/
https://warmglass.com/what-caused-this-huge-bubble/
- Wed Sep 14, 2022 3:43 pm
- Forum: Techniques and Tools
- Topic: Bubble
- Replies: 2
- Views: 9505
Bubble
I'm sometimes getting a large bubble when fusing this piece, the long dimension is 12 inches. Fired on Papyros, my usual full-fuse program that works fine with smaller pieces, and sometimes works fine with this size. Any ideas what causes this?
- Wed Sep 07, 2022 3:57 pm
- Forum: Techniques and Tools
- Topic: Tack fused 24x24 not flat
- Replies: 3
- Views: 13311
Re: Tack fused 24x24 not flat
I had a similar problem ... Youghiogheny 96, piece was about 10 x 12 inches. After full fuse it seemed not quite flat. It broke in half during a slump fire - sometime during the anneal or cool down - the shape was correct, just in 2 pieces now. Maybe incompatible glass - the top layer is Y96-7937M w...
- Wed Aug 24, 2022 10:01 am
- Forum: Techniques and Tools
- Topic: Gloves
- Replies: 3
- Views: 15438
Re: Gloves
Mine came from Home Depot, in the tools section. They're marked "Premium Defense." Thinner than gardening gloves. Much thicker than latex or medical gloves - I wouldn't expect these to provide any protection from glass as they're designed to block dirt, bacteria and viruses.
- Fri May 15, 2020 3:59 pm
- Forum: Newcomer Forum
- Topic: Controlling my new Bartlet controller
- Replies: 1
- Views: 12509
Re: Controlling my new Bartlet controller
Assuming you have the color touch screen controller ...
First load the program you want to change
Then touch Edit
From here you can touch the value you want to change and it should prompt for the new value.
Remember to save it when you're done.
Hope this helps
First load the program you want to change
Then touch Edit
From here you can touch the value you want to change and it should prompt for the new value.
Remember to save it when you're done.
Hope this helps